Celanese Celanex® 3214 15% Fiberglass Reinforced Polybutylene Terephthalate
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic; Polymer
Material Notes: Description: Celanex 3214 is a non-exuding (UL approved V-0 at 1/32 inch), 15% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability. It is well suited for electrical connector applications. Data provided by Ticona.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Rockwell M
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Back Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|