Celanese Celanex® 3114 7.5% Fiberglass Reinforced Polybutylene Terephthalate
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic; Polymer
Material Notes: Description: Celanex 3114 is a flame retarded, nonexuding, 7.5% glass reinforced polybutylene terephthalate providing a good balance of mechanical and electrical properties. This grade is rated UL94 V-0 down to 1/32 inch thickness and is recommended for all electrical/electronic applications. Data provided by Ticona.
| Available Properties |
- Density
- Tensile Strength at Break
- Tensile Modulus
- Flexural Modulus
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Melting Point
- Flammability, UL94
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Back Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|