Celanese Celcon® M25HT High Impact Acetal Copolymer
Subcategory: Acetal; Thermoplastic
Material Notes: Description: Celcon M25HT is an extraordinarily tough acetal copolymer formulated for very high impact properties. It has a high melt strength for extrusion and blow molding applications, while still being injection moldable. Data provided by Ticona.
| Available Properties |
- Density
- Tensile Strength, Yield
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
|
|
|
|
| Property Data |