Celanese Celcon® TX86 Ductile Acetal Copolymer
Subcategory: Acetal; Thermoplastic
Material Notes: Description: Celcon TX86 is a slightly toughened acetal copolymer which exhibits ductility in bending and impact loading. The ductile rather than brittle, failure mode gives engineers greater design freedom in applications such as clips, fasteners, gears and rollers. Data provided by Ticona.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Yield
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
|
|
|
|