Celanese Celcon® CF802 Dissipative, Fuel Compatible General Purpose Material
Subcategory: Acetal; Thermoplastic
Material Notes: Description: Celcon CF802 is a dissipative, fuel compatible general purpose material which has typical surface resistivity of 1000 ohms, volume resistivity of 10 ohm-meters (1000 ohm-cm) and static decay rate of 0.01 seconds or less. Data provided by Ticona.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Yield
- Tensile Modulus
- Charpy Impact, Notched
- Volume Resistivity
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|