Celanese Celcon® LM90 Acetal Copolymer (Capable of being Laser Marked)
Subcategory: Acetal; Thermoplastic
Material Notes: Description: Celcon LM90 is a 9.0 melt flow rate acetal copolymer which is capable of being permanently marked by a laser. Parts molded from Celcon LM90 can be laser marked with barcodes, ID numbers and designs. Data provided by Ticona.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Yield
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
|
|
|
|