Celanese Celcon® LM25 Acetal Copolymer (Capable of being Laser Marked)
Subcategory: Acetal; Thermoplastic
Material Notes: Description: Celcon LM25 is a 2.5 melt flow acetal copolymer which is capable of being permanently marked by a laser. Parts molded from Celcon LM25 can be lasermarked with bar-codes, identification numbers, designs, 2-D symbology, etc. Data provided by Ticona.
| Available Properties |
- Density
- Tensile Strength, Yield
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|