Celanese Celcon® C13031 XF Acetal Copolymer
Subcategory: Acetal; Thermoplastic
Material Notes: Description: Celcon acetal copolymer grade C13031 XF is a general purpose acetal copolymer, modified to resist deterioration from hot oxidized fuels including diesel, and bio-diesel fuels. This material is specially targeted for transportation industry fuel systems. Celcon C13031 XF is a dark yellow color to denote use for fuel systems. Data provided by Ticona.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Tensile Modulus
- Charpy Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
|
|
|
|