Celanese Celcon® WR25HT High Impact Acetal Copolymer
Subcategory: Acetal; Thermoplastic
Material Notes: Description: Celcon WR25HT is a black, weather resistant, extraordinarily tough acetal copolymer formulated for very high impact properties, It has high melt strength for extrusion and blow molding applications, while still being injection moldable. Data provided by Ticona.
| Available Properties |
- Density
- Tensile Strength, Yield
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature