Celanese Fortron® 9320C0 Polyphenylene Sulfide (PPS)
Subcategory: Polyphenylene Sulfide; Thermoplastic
Material Notes: Description: Fortron 9320C0 is an unfilled grade for extrusion applications which demonstrates excellent chemical resistance and thermal stability. Components made of this grade may be used for medical and food handling applications. Fortron 9320C0 is in compliance with ISO 10993, USP Class VI, and is included in the Fortron Drug and Device Master Files at the FDA. This grade complies with the FDA Food Contact Notification (FCN-No. 40) for repeat-use applications. Data provided by Ticona.
| Available Properties |
- Density
- Water Absorption at Saturation
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched (ISO)
- Volume Resistivity
- Dielectric Constant
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Glass Temperature
- Melt Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|