Celanese Fortron® 1140L0 40% Glass Reinforced Polyphenylene Sulfide (PPS)
Subcategory: Polyphenylene Sulfide; Thermoplastic; Polymer
Material Notes: Description: Fortron 1140L0 is a 40% glass-reinforced extrusion grade. It exhibits excellent heat and chemical resistance, good electrical properties and is inherently flame-retardant. The high hardness and rigidity at elevated temperatures allows for good load bearing performance. This product has good weldability due to the modest filler level. 1140L0 is used to produce rods and slabs. Data provided by Ticona.
| Available Properties |
- Density
- Water Absorption at Saturation
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Melting Point
- Glass Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|