Celanese Fortron® 1140EC Glass Reinforced Polyphenylene Sulfide (PPS)
Subcategory: Polyphenylene Sulfide; Thermoplastic; Polymer
Material Notes: Description: Fortron 1140EC offers a unique balance of properties based on a glass reinforced composition, complementing our other fiberglass reinforced product offerings. As with all Fortron grades this product is inherently flame-retardant. Applications include automotive engine cooling components. Data provided by Ticona.
| Available Properties |
- Density
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Rockwell M
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched (ISO)
- Volume Resistivity
- Dielectric Constant
- Dissipation Factor
- Comparative Tracking Index
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|