Celanese Fortron® 6160B4 Polyphenylene Sulfide (PPS)
Subcategory: Polyphenylene Sulfide; Thermoplastic
Material Notes: Description: Fortron 6160B4 has excellent heat and chemical resistance as well as good electrical properties. This product is inherently flame-retardant and offers high hardness and rigidity. 6160B4 has demonstrated excellent performance in hot runner systems and superior contact corrosion resistance. Applications include electronic components (i.e. molded in lead frames, contacts or pins). Data provided by Ticona.
| Available Properties |
- Density
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Rockwell M
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Glass Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|