Celanese Impet® Hi430 15% Glass Filled, Impact Modified PET
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic; Polymer
Material Notes: Description: Impet Hi 430 is a 15% glass filled and impact modified PET which has an excellent balance of mechanical properties as well as excellent processability and surface appearance. Data provided by Ticona.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength at Break
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Tensile Modulus
- Flexural Modulus
- Flexural Modulus
- Flexural Strength
- Flexural Yield Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Izod Impact, Notched
- Dielectric Strength
- Arc Resistance
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Back Pressure
|
|
|
|
| Property Data |
This page displays only the text