Celanese Riteflex® 635 Thermoplastic Polyester Elastomer (TPE)
Subcategory: Polyester, TP; Thermoplastic; Polyester TPE
Material Notes: Description: 35 Shore D Hardness 8,800 PSI flexural modulus Data provided by Ticona.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Tensile Modulus
- 50% Modulus
- Flexural Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Tear Strength
- Izod Impact, Notched
- Izod Impact, Notched @ -40°C
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Injection Pressure
- Back Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|