Celanese Vandar® AB200 Low Modulus Polyester Alloy
Subcategory: Polyester, TP; Thermoplastic
Material Notes: Description: Vandar AB200 is a low modulus polyester alloy which exhibits excellent toughness and impact strength. It is typically used for driver airbag covers. Data provided by Ticona.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- 50% Modulus
- Flexural Modulus
- Flexural Modulus
- Flexural Strength
- Flexural Yield Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 0.46 MPa (66 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Back Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|