Celanese Vandar® 2100UV High Impact Polyester Alloy
Subcategory: Polyester, TP; Thermoplastic
Material Notes: Description: Vandar 2100UV is a polyester alloy designed to offer maximum impact strength at room and low temperatures. This unfilled compound is characterized by outstanding chemical resistance, dimensional stability, paintability, and toughness. Vandar 2100UV is available in UV stable colors. Data provided by Ticona.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell M
- Tensile Strength, Yield
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- 50% Modulus
- Flexural Modulus
- Flexural Modulus
- Flexural Strength
- Flexural Yield Strength
- Izod Impact, Notched (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Izod Impact, Notched
- Izod Impact, Notched @ -30°C
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
- Back Pressure
|
|
|
|
| Property Data |
This page displays only the text