Celanese GmbH Hostaform C 13021 K Acetal Copolymer with Special Chalk
Subcategory: Acetal; Thermoplastic; Polymer
Material Notes: Description: Hostaform® Acetal Copolymers are a high strength, crystalline, thermoplastic engineering resins whose balance of properties and ease of processability offer performance and cost advantages over many other materials. Hostaform Acetal Copolymers are manufactured and marketed by Ticona GmbH, the European division of Ticona. Specific Notes for this Grade: Easy flowing injection molding grade modified with special chalk. Good antiwear properties, increased strength. For unlubricated or once-only lubricated sliding elements.Information provided by Ticona.
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|