Celanese GmbH Hostaform S 27072 WS 10/1570 Elastomer Modified, Weather Resistant Acetal Copolymer
Subcategory: Acetal; Thermoplastic
Material Notes: Description: Hostaform® Acetal Copolymers are a high strength, crystalline, thermoplastic engineering resins whose balance of properties and ease of processability offer performance and cost advantages over many other materials. Hostaform Acetal Copolymers are manufactured and marketed by Ticona GmbH, the European division of Ticona. Specific Notes for this Grade: Easy flowing injection molding grade, elastomer-modified and weathering-resistant. For durable matt surfaces in outdoor applications.Information provided by Ticona.
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Melt Flow
- Ball Indentation Hardness
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Penetration
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|