Celanese GmbH Hostaform MT 8R02 Acetal Copolymer
Subcategory: Acetal; Thermoplastic
Material Notes: Description: Hostaform® Acetal Copolymers are a high strength, crystalline, thermoplastic engineering resins whose balance of properties and ease of processability offer performance and cost advantages over many other materials. Hostaform Acetal Copolymers are manufactured and marketed by Ticona GmbH, the European division of Ticona. Specific Notes for this Grade: Injection molding grade, good flowability, good combination of mechanical and tribological properties, specially manufactured for healthcare applications. With this grade, Ticona offers a consistent quality and material formulations unchanging over a long period of time. Through extensive testing of individual lots, a very high level of product quality is achieved for OEMs and molders.Information provided by Ticona.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- BgVV Recommendations
- Consumer Articles Regulations
- Device Master File
- Drug Master File
- FDA Regulation CFR Vol21S177
- ISO 10993
- USP 23 Class VI
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|