Celanese GmbH Hostaform C 27021 XAP Acetal Copolymer
Subcategory: Acetal; Thermoplastic
Material Notes: Description: Hostaform® Acetal Copolymers are a high strength, crystalline, thermoplastic engineering resins whose balance of properties and ease of processability offer performance and cost advantages over many other materials. Hostaform Acetal Copolymers are manufactured and marketed by Ticona GmbH, the European division of Ticona. Specific Notes for this Grade: Ticona had already launched low odor injection molding grades in 1998. These Hostaform grades have been given the code XAP, with X standing for innovative development products and AP for Advanced Processing.Information provided by Ticona.
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Melt Flow
- Ball Indentation Hardness
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Emission
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|