PolyOne Edgetek® MLS-20GF/000 Polysulfone Alloy - 20% Glass Fiber Reinforced
Subcategory: Polysulfone; Thermoplastic; Polymer
Close Analogs: This product is no longer a part of the PolyOne standard product line.
Material Notes: Data provided by PolyOne.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength @ Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Melt Temperature
|
|
|
|
| Property Data |