PolyOne Elastamax® XL 0117-5 SEBS-Based Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic
Close Analogs: This product is no longer a part of the PolyOne standard product line.
Material Notes: This is a general purpose elastamax based on SEBS technology. It offers good compression set resistance and is intended for food contact applications. Physical Form: Pellet. Standard Color: Translucent. Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 50% Modulus
- 100% Modulus
- 200% Modulus
- 300% Modulus
- Tear Strength
- Compression Set
- Compression Set, Elevated Temperature
- Tensile Set
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|