PolyOne Elastamax® XL 0168-40 SEBS-Based Thermoplastic Elastomer
  Subcategory: Elastomer, TPE; Thermoplastic 
Close Analogs: This product is no longer a part of the PolyOne standard product line. 
Material Notes:  This is a modified SEBS elastomer compound tailored for adhesion to PPO.  Physical Form: Pellet.  Standard Color: Grey to black.  13.8 pli overmold adhesion to PPO. Information provided by M. A. Hanna.  M. A. Hanna and Geon merged to form PolyOne in 2000.    
  
  
    | Available Properties | 
   
    
    - Density
 
- Linear Mold Shrinkage
 
- Melt Flow
 
- Hardness, Shore A
 
- Tensile Strength, Ultimate
 
- Elongation at Break
 
- 50% Modulus
 
- 100% Modulus
 
- 200% Modulus
 
- 300% Modulus
 
- Tear Strength
 
 
   |   
   |   
 | 
   | 
  
  
    | Property Data | 
   
    