PolyOne Elastamax® XL 0201-2 Polypropylene Compound
Subcategory: Polypropylene; Thermoplastic
Close Analogs: This product is no longer a part of the PolyOne standard product line.
Material Notes: This is a conductive polypropylene copolymer compound. Physical Form: Pellet. Standard Color: Grey. Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000.