|   PolyOne Elastamax® XL 0240-1 TPO-Based Thermoplastic Elastomer  Subcategory: Elastomer, TPE; Thermoplastic Close Analogs: This product is no longer a part of the PolyOne standard product line. Material Notes: This is a general purpose elastomer based on TPO technology.  It exhibits low modulus and is modified with a flame retardant additive.  Physical Form: Pellet.  Standard Color: Black.
 Information provided by M. A. Hanna.  M. A. Hanna and Geon merged to form PolyOne in 2000.    
| | 
    | Available Properties |  
    | DensityMelt FlowHardness, Shore ATensile Strength, UltimateElongation at Break50% Modulus100% ModulusTear Strength
 | 
 | 
 |  | | 
    | Property Data |  
    | 