Degussa AG Europlex® F4 Transparent Flame Retardant Sheet
Subcategory: Thermoplastic
Material Notes: Description: EUROPLEX® F4 is a flame retardant sheet material as well as EUROPLEX® F3, but transparent. Therefore this material can be used for smaller cabin interior parts like lighting fixture covers, emergency lighting system and other similar applications. Applications: - lighting covers
- back lighted signs
- Emergency lighting systems
- interior glazing
Information provided by degussa.