Degussa AG Europlex® F6 White-Translucent Sheet
Subcategory: Thermoplastic
Material Notes: Description: EUROPLEX® F6 is a flame-retarded, white-translucent material that is specially suited for light covers in aircraft cabins. Applications: lighting covers Information provided by degussa.
| Available Properties |
- Density
- Tensile Strength at Break
- Elongation at Break
- Modulus of Elasticity
- Charpy Impact Unnotched
- Maximum Service Temperature, Air
- Vicat Softening Point
|
|
|
|