Degussa AG Europlex® Film 99510 Transparent Polycarbonate Based Film
Subcategory: Polycarbonate; Thermoplastic; Polymer
Material Notes: Description: EUROPLEX® Film 99510 is a highly transparent film made from polycarbonate with special UV stabilization. It has a high-gloss surface, is inherently rigid and highly impact-resistant in a temperature range between -25 °C and 135 °C. It is resistant to weak acids and saturated aliphatic hydrocarbons. Specific Notes for this Material: EUROPLEX® Film 99510 is employed for scales, nameplates, signs, covers, glazing, safety helmet shells, protective goggles and visors as well as for model making. Information provided by degussa.
| Available Properties |
- Density
- Film Tensile Strength at Yield, MD
- Film Elongation at Break, MD
- Film Elongation at Yield, MD
- Tensile Modulus
- Volume Resistivity
- Surface Resistance
- Dissipation Factor
- Dissipation Factor, Low Frequency
- CTE, linear 20°C
- Specific Heat Capacity
- Vicat Softening Point
- Haze
- Yellow Index
- Transmission, Visible
- Birefringence
- Pencil Hardness
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|