Degussa AG Europlex® HC 99710 PMMA Based Transparent Film
Subcategory: Acrylic; Thermoplastic; Polymer; Polymethacrylimide
Material Notes: Description: EUROPLEX® Film HC 99710 is a highly transparent, very efficient weather and UV protection film with excellent surface properties such as chemical resistance, antigraffiti and dirt-repellent behavior. EUROPLEX® Film HC 99710 is based on a special polymethyl methacrylate (PMMA) formulation with outstanding weather resistance, extremely high UV absorption as well as superior printability and lamination performance. It owes these extraordinary surface properties to the polyvinylidene fluoride (PVDF) layer which is fused to the PMMA substrate. Specific Notes for this Material: EUROPLEX® Film HC 99710 is suitable for protecting and upgrading the surfaces of sheets and films made from PVC, PC or ABS, for example. Moreover, it can be employed as a cap layer film on textiles, wood, laminated plastics and metals. The film is used for exterior and interior applications in buildings, in exterior automotive body parts and automotive interior trim. Information provided by degussa.
| Available Properties |
- Density
- Surface Tension
- Film Tensile Strength at Yield, MD
- Film Elongation at Break, MD
- Tensile Modulus
- Haze
- Yellow Index
- Transmission, Visible
- UV Transmittance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|