Degussa AG Europlex® HC 99710 PMMA Based Transparent Film

 

Subcategory: Acrylic; Thermoplastic; Polymer; Polymethacrylimide

Material Notes:
Description: EUROPLEX® Film HC 99710 is a highly transparent, very efficient weather and UV protection film with excellent surface properties such as chemical resistance, antigraffiti and dirt-repellent behavior. EUROPLEX® Film HC 99710 is based on a special polymethyl methacrylate (PMMA) formulation with outstanding weather resistance, extremely high UV absorption as well as superior printability and lamination performance. It owes these extraordinary surface properties to the polyvinylidene fluoride (PVDF) layer which is fused to the PMMA substrate.

Specific Notes for this Material: EUROPLEX® Film HC 99710 is suitable for protecting and upgrading the surfaces of sheets and films made from PVC, PC or ABS, for example. Moreover, it can be employed as a cap layer film on textiles, wood, laminated plastics and metals. The film is used for exterior and interior applications in buildings, in exterior automotive body parts and automotive interior trim.

Information provided by degussa.

Available Properties
  • Density
  • Surface Tension
  • Film Tensile Strength at Yield, MD
  • Film Elongation at Break, MD
  • Tensile Modulus
  • Haze
  • Yellow Index
  • Transmission, Visible
  • UV Transmittance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。