Degussa AG Europlex® PPSU Polyphenylsulfone Engineering Plastic

 

Subcategory: Polyphenylsulfone; Thermoplastic

Material Notes:
Description: EUROPLEX® PPSU is a sheet material distinguished by its special combination of properties:

  • high heat distortion temperature up to 190° C in permanent service
  • EUROPLEX® PPSU has outstanding mechanical properties over a wide temperature range (also at very low temperatures)
  • EUROPLEX® PPSU shows extraordinary chemical resistance for an amorphous material
  • Parts made of EUROPLEX® PPSU can be sterilized by all conventional methods, particularly by superheated steam at 2,000 cycles or more, also in combination with morpholine
  • EUROPLEX® PPSU therefore shows very particularly good resistance to hydrolysis
  • EUROPLEX® PPSU is inherently flame-retarded. Its rating to UL94:VO at 1.6 mm thickness stands for very good fire behavior
  • EUROPLEX® PPSU is physiologically unobjectionable and easily meets FDA and USP requirements for food contact and medical applications
  • Available in the form of transparent or opaque sheets in thicknesses of 0.8 to 6.0 mm
  • Sheets made from this material are mainly processed into medical containers for use in hospitals. Beside this EUROPLEX® PPSU sheets are more and more used in industrial plants and machines

Information provided by degussa.

Available Properties
  • Density
  • Tensile Strength at Break
  • Modulus of Elasticity
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Maximum Service Temperature, Air
  • Vicat Softening Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。