Degussa AG Europlex® PPSU Polyphenylsulfone Engineering Plastic
Subcategory: Polyphenylsulfone; Thermoplastic
Material Notes: Description: EUROPLEX® PPSU is a sheet material distinguished by its special combination of properties:- high heat distortion temperature up to 190° C in permanent service
- EUROPLEX® PPSU has outstanding mechanical properties over a wide temperature range (also at very low temperatures)
- EUROPLEX® PPSU shows extraordinary chemical resistance for an amorphous material
- Parts made of EUROPLEX® PPSU can be sterilized by all conventional methods, particularly by superheated steam at 2,000 cycles or more, also in combination with morpholine
- EUROPLEX® PPSU therefore shows very particularly good resistance to hydrolysis
- EUROPLEX® PPSU is inherently flame-retarded. Its rating to UL94:VO at 1.6 mm thickness stands for very good fire behavior
- EUROPLEX® PPSU is physiologically unobjectionable and easily meets FDA and USP requirements for food contact and medical applications
- Available in the form of transparent or opaque sheets in thicknesses of 0.8 to 6.0 mm
- Sheets made from this material are mainly processed into medical containers for use in hospitals. Beside this EUROPLEX® PPSU sheets are more and more used in industrial plants and machines
Information provided by degussa.
| Available Properties |
- Density
- Tensile Strength at Break
- Modulus of Elasticity
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Maximum Service Temperature, Air
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|