Degussa Plexiglas® 99526 Crystal Clear Elastomer Based Film
Subcategory: Acrylic; Thermoplastic; Polymer
Material Notes: Description: PLEXIGLAS® Film 99526, based on polymethyl methacrylate and acrylic elastomers, is absolutely crystal-clear. With its excellent abrasion resistance, it offers outstanding performance as a decor carrier and for substrate protection. Moreover, it shows very good weather resistance, two glossy surfaces and has no surface markings (Class A surface). In addition, it presents good resistance towards weak acids and alkalis as well as nonpolar solvents. Specific Notes for this Material: PLEXIGLAS® Film 99526 is particularly suitable for decorative and protective surfaces of injection molded parts for the automotive, domestic appliances and telecommunications sectors. This film is eminently suitable for all in-mold film decoration processes. In thicknesses of 60 to 75 µm; PLEXIGLAS® Film 99526 serves very well as a hard cap layer film in multiply lamination film systems or on extruded plastic sheets. Information provided by degussa.
| Available Properties |
- Density
- Film Tensile Strength at Yield, MD
- Film Elongation at Break, MD
- Film Elongation at Yield, MD
- Tensile Modulus
- Volume Resistivity
- Surface Resistance
- Dissipation Factor
- Dissipation Factor, Low Frequency
- CTE, linear 20°C
- Specific Heat Capacity
- Vicat Softening Point
- Refractive Index
- Haze
- Yellow Index
- Transmission, Visible
- UV Transmittance
- Pencil Hardness
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|