Degussa Plexiglas® df23 8N Molding Compound

 

Subcategory: Acrylic; Thermoplastic

Material Notes:
Description: PLEXIGLAS® df21 8N, PLEXIGLAS® df22 8N and PLEXIGLAS® df23 8N molding compounds based on PLEXIGLAS® 8N are characterized by diffuse scattering of light. Besides showing the familiar properties of standard PLEXIGLAS® molding compound, such as

  • excellent weatherability
  • high surface hardness and scratch resistance

PLEXIGLAS® df21 8N, PLEXIGLAS® df22 8N and PLEXIGLAS® df23 8N are special in that they combine good diffusing power with excellent light transmission.

PLEXIGLAS df molding compounds are the optimal choice, when a combination of high light scattering and excellent light transmission is required. Both, PLEXIGLAS df22 8N and PLEXIGLAS df23 8N are well designed for lamp covers, projected areas and similar applications. For displays and backlight units PLEXIGLAS df21 8N is the favored material.

Information provided by degussa.

Available Properties
  • Density
  • Melt Flow
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Charpy Impact Unnotched
  • CTE, linear 20°C
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Glass Temperature
  • Glow Wire Test
  • Transmission, Visible
  • Processing Temperature
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  • Energy Half Angle
  • Fire Rating
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。