Degussa Plexiglas® GS 249 Cast Acrylic
Subcategory: Acrylic; Thermoplastic
Material Notes: Description: PLEXIGLAS® GS 249 is another cast acrylic specially developed to meet even higher demands by the aviation industry, but is additionally crosslinked. As compared with uncrosslinked acrylic, it offers higher resistance to media that cause stress cracking and increased heat distortion resistance. PLEXIGLAS® GS 249 is also excellently suited for stretching, which makes it possible to improve its properties even further over the unstretched state. Typical applications are cabin windows in civilian aircraft, glazing for pressurized aircraft cabins, cockpit glazing, canopies and windshields. Information provided by degussa.
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Tensile Strength at Break
- Elongation at Break
- CTE, linear 20°C
- Maximum Service Temperature, Air
- Vicat Softening Point
- Refractive Index
- Haze
- Transmission, Visible
- UV Transmittance
- Angular Deviation
- Fire Rating
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|