Degussa Plexiglas® hw55 Clear Molding Compound
Subcategory: Acrylic; Thermoplastic
Material Notes: Description: PLEXIGLAS® hw55 clear is a copolymer based on methyl methacrylate (MMA) with comonomer constituents. Besides showing the familiar properties of standard PLEXIGLAS® molding compound, such as- high light transmission
- good flowability
- high mechanical strength, surface hardness and abrasion resistance
- excellent weatherability
PLEXIGLAS® hw55 clear offers the additional benefits of - increased heat deflection temperature under load
- improved resistance to stress cracking
- optimized inherent color
PLEXIGLAS® hw55 clear is particularly suitable for injection molding of technical items. Uses of PLEXIGLAS® hw55 clear: lighted keys, luminaire covers, fiber optics. Information provided by degussa.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Melt Flow
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Glass Temperature
- Flammability, UL94
- Refractive Index
- Transmission, Visible
- Processing Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|