Degussa Plexiglas® Soundstop® GS Extruded Acrylic
Subcategory: Acrylic; Thermoplastic
Material Notes: Description: PLEXIGLAS® GS cast acrylic has the following properties:- absolutely colorless and clear
- break-resistant
- unequalled resistance to weathering and ageing
- high-quality surface and planarity; brilliant or satin (PLEXIGLAS SATINICE®)
- sheets, blocks, tubes, round and square rods
- 2 to 160 mm solid sheet / block thickness
- standard size up to 3050 x 2030 mm
- more than 50 standard colors
- good resistance to dilute acids
- limited resistance to organic solvents
- good resistance to alkalis
- very easy to work, similar to hardwood
- easy to thermoform over wide range of conditions
- easily and firmly bonded, e.g. with reaction adhesives (e.g. ACRIFIX® 190, 192)
- burns more or less like hardwood; very little smoke generation
- max. service temperature approx. 80 °C
Specific Notes for this Material: Flame-retarded, UV absorbing solid sheet special grade in accordance with ZTV-Lsw 88, EN 1793 and EN 1794 for noise control barriers. Information provided by degussa.
| Available Properties |
- Density
- Tensile Strength at Break
- Modulus of Elasticity
- Flexural Strength
- Fatigue Strength
- Shielding Effectiveness
- CTE, linear 20°C
- Vicat Softening Point
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|