Degussa Plexiglas® Superclear 99560 Extruded PMMA Sheet
Subcategory: Acrylic; Thermoplastic
Material Notes: Description: PLEXIGLAS® Superclear 99560 is an extruded PMMA product that has been developed for applications with highest demands on optical and surface quality. It has no observable haze, a very smooth surface and no light absorption. The material is best suited for hard coating. Information provided by degussa.
| Available Properties |
- Density
- Water Absorption at Saturation
- Moisture Vapor Transmission
- Ball Indentation Hardness
- Tensile Strength at Break
- Tensile Strength, Ultimate at Elevated Temperature
- Elongation at Break
- Modulus of Elasticity
- Flexural Strength
- Compressive Yield Strength
- Izod Impact, Notched (ISO)
- Charpy Impact Unnotched
- Coefficient of Friction
- Abrasion
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Flash Point
- Refractive Index
- Haze
- Transmission, Visible
- UV Transmittance
- Reflection Coefficient, Visible (0-1)
- Processing Temperature
- Absorption in the Visible Range
- Number of Inclusions (0.1 mm to 0.25 mm)
- Number of Inclusions (0.25 mm to 0.65 mm)
- Number of Inclusions (0.65 mm to 1.65 mm)
- Pencil Hardness
- Permeability to Air
- Permeability to CO2
- Permeability to N2
- Permeability to O2
- Sound Velocity
- Total Energy Transmittance
- U Value for 10mm
- U Value for 1mm
- U Value for 3mm
- U Value for 5mm
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|