Degussa Plexiglas® XT 20070 Extruded Acrylic

 

Subcategory: Acrylic; Thermoplastic

Material Notes:
Description: PLEXIGLAS® XT extruded acrylic has the following properties:

  • absolutely colorless and clear
  • break-resistant to impact-resistant (PLEXIGLAS RESIST®)
  • unequalled resistance to weathering and ageing
  • very good surface; brilliant, textured or satin (PLEXIGLAS SATINICE®)
  • sheets, tubes, round rods, multi-skin sheets, corrugated sheets, mirror sheets
  • 1.5 to 25 mm solid sheet thickness, multi-skin sheets 16 mm and 32 mm thick
  • standard size up to 4050 x 2050 mm (+ extra lengths)
  • more than 25 standard colors
  • good resistance to dilute acids
  • limited resistance to organic solvents
  • good resistance to alkalis
  • easy to work, similar to hardwood
  • easy to thermoform under optimal constant conditions
  • easily bonded also with solvent adhesives (e.g. ACRIFIX® 116, 117)
  • burns more or less like hardwood; very little smoke generation
  • max. service temperature approx. 70 °C

Specific Notes for this Material: Standard grade for solid sheets; largely UV-absorbing.

Information provided by degussa.

Available Properties
  • Density
  • Water Absorption
  • Water Absorption at Saturation
  • Moisture Expansion
  • Moisture Vapor Transmission
  • Ball Indentation Hardness
  • Tensile Strength at Break
  • Tensile Strength, Ultimate at Elevated Temperature
  • Elongation at Break
  • Modulus of Elasticity
  • Flexural Strength
  • Compressive Yield Strength
  • Poissons Ratio
  • Shear Modulus
  • Izod Impact, Notched (ISO)
  • Charpy Impact Unnotched
  • Impact
  • Coefficient of Friction
  • Abrasion
  • Volume Resistivity
  • Surface Resistance
  • Shielding Effectiveness
  • Dielectric Constant
  • Dielectric Constant, Low Frequency
  • Dielectric Strength
  • Dissipation Factor
  • Dissipation Factor, Low Frequency
  • Comparative Tracking Index
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Flash Point
  • Refractive Index
  • Transmission, Visible
  • UV Transmittance
  • Reflection Coefficient, Visible (0-1)
  • Processing Temperature
  • Adsorption in the Visible Range
  • Fire Rating
  • Min Cold Bending Radius
  • Permeability to Air
  • Permeability to CO2
  • Permeability to N2
  • Permeability to O2
  • Sound Velocity
  • Total Energy Transmittance g
  • U Value for 10mm
  • U Value for 1mm
  • U Value for 3mm
  • U Value for 5mm
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。