Degussa Plexiglas® XT 29070 Extruded Acrylic
Subcategory: Acrylic; Thermoplastic
Material Notes: Description: PLEXIGLAS® XT extruded acrylic has the following properties:- absolutely colorless and clear
- break-resistant to impact-resistant (PLEXIGLAS RESIST®)
- unequalled resistance to weathering and ageing
- very good surface; brilliant, textured or satin (PLEXIGLAS SATINICE®)
- sheets, tubes, round rods, multi-skin sheets, corrugated sheets, mirror sheets
- 1.5 to 25 mm solid sheet thickness, multi-skin sheets 16 mm and 32 mm thick
- standard size up to 4050 x 2050 mm (+ extra lengths)
- more than 25 standard colors
- good resistance to dilute acids
- limited resistance to organic solvents
- good resistance to alkalis
- easy to work, similar to hardwood
- easy to thermoform under optimal constant conditions
- easily bonded also with solvent adhesives (e.g. ACRIFIX® 116, 117)
- burns more or less like hardwood; very little smoke generation
- max. service temperature approx. 70 °C
Specific Notes for this Material: Standard grades for multiskin sheets PLEXIGLAS® S4P 32 and PLEXIGLAS ALLTOP® SDP 16, tubes and round rods, UV transmitting. Information provided by degussa.
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Moisture Expansion
- Moisture Vapor Transmission
- Ball Indentation Hardness
- Tensile Strength at Break
- Tensile Strength, Ultimate at Elevated Temperature
- Elongation at Break
- Modulus of Elasticity
- Flexural Strength
- Compressive Yield Strength
- Poissons Ratio
- Shear Modulus
- Izod Impact, Notched (ISO)
- Charpy Impact Unnotched
- Impact
- Coefficient of Friction
- Abrasion
- Volume Resistivity
- Surface Resistance
- Shielding Effectiveness
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flash Point
- Refractive Index
- Transmission, Visible
- UV Transmittance
- Reflection Coefficient, Visible (0-1)
- Processing Temperature
- Adsorption in the Visible Range
- Fire Rating
- Min Cold Bending Radius
- Permeability to Air
- Permeability to CO2
- Permeability to N2
- Permeability to O2
- Sound Velocity
- Total Energy Transmittance g
- U Value for 10mm
- U Value for 1mm
- U Value for 3mm
- U Value for 5mm
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|