Degussa Plexiglas® zk6HC Molding Compound
Subcategory: Acrylic; Thermoplastic
Material Notes: Description: PLEXIGLAS® zk4HC, PLEXIGLAS® zk5HC and PLEXIGLAS® zk6HC are impact-modified molding compounds. Besides showing the familiar properties of basic PLEXIGLAS® molding compound, such as- high break resistance and impact strength
- excellent weatherability
- high surface hardness and abrasion resistance
PLEXIGLAS® zk HC molding compounds offer the added benefit of being the most highly craze-resistant impact-modified PLEXIGLAS® molding compounds. PLEXIGLAS® zk molding compounds of the HC series are suitable for extrusion and coextrusion of sheets and profiles. Uses of PLEXIGLAS® zkHC molding compounds: extruded/coextruded sheets and profiles for automotive bodies and the sanitary sector (bathtubs and shower tubs) or crystal-clear lighting fixture covers for industrial plants that come into contact with aggressive media. Information provided by degussa.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- CTE, linear 20°C
- Vicat Softening Point
- Flammability, UL94
- Refractive Index
- Transmission, Visible
- Processing Temperature
- Die Temperature
- Melt Temperature
- Drying Temperature
- Dry Time
- Fire Rating
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|