Degussa Plexiglas® zk6HF Molding Compound
Subcategory: Acrylic; Thermoplastic
Material Notes: Description: PLEXIGLAS® zk5HF and PLEXIGLAS® zk6HF are impact-modified molding compounds based on the PLEXIGLAS® zkBR series. Besides showing the familiar properties of basic PLEXIGLAS® molding compound, such as- high break resistance and impact strength
- excellent weatherability
- high surface hardness and abrasion resistance
PLEXIGLAS® zkHF molding compounds offer the added benefit of very good flow properties. PLEXIGLAS® zk molding compounds of the HF series are suitable for injection molding as well as for extrusion of sheets and profiles. Uses of PLEXIGLAS® zkHF molding compounds: applications involving long flow paths through narrow channels, thin-walled component parts; items requiring accurate mold surface reproduction, such as very finely textured luminaire covers. Information provided by degussa.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- CTE, linear 20°C
- Vicat Softening Point
- Flammability, UL94
- Refractive Index
- Transmission, Visible
- Processing Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Fire Rating
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|