Degussa AG Vestamelt® 351 Copolyamide Hotmelt Adhesive
Subcategory: Adhesive; Nylon; Thermoplastic
Material Notes: Description: High Performance Polymers manufactures a line of customized hotmelt adhesives. They are supplied as powders and granulates under the trade name VESTAMELT®. Used in a variety of industries, they provide all applications with a good balance of high-quality service properties, easy and reliable processing, and high cost-effectiveness. VESTAMELT® features the following special properties:- economic bonding, also to sensitive textiles and surfaces that are difficult to fuse
- high resistance to washing and dry cleaning
- good resistance to strike back steam resistance
- solvent resistance
VESTAMELT® powders or granulates can be applied to substrates by means of typical processes. VESTAMELT® hotmelt adhesives are used in various application fields: - In the textile industry they bond interlinings in women’s and men’s garments. In addition, they are successfully used in technical textile manufacturing.
- The automotive industry uses the thermoplastic hotmelt adhesives to fix interior trim and seat heaters on the one hand, on the other hand for the reliable bonding of paper to aluminum for the construction of fuel filters.
- Copolyamide hotmelt adhesives permit cost-effective manufacture of advanced components as windows, ceilings, carpets and acoustic insulation systems with lightweight panels.
- To make deflection yokes, insulated wires are coated with hotmelt varnishes and bonded together. The dimensionally stable coils obtained in this way find application in the electrical industry.
Information provided by degussa.
| Available Properties |
- Viscosity Measurement
- Melt Flow
- Melting Point
- Heat Setting Pressure
- Heat Setting Temperature
- Heat Setting Time
- Resistance to Dry Cleaning
- Resistance to Steam
- Resistance to Washing at 60°C
- Supply Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|