Degussa AG Solimide® AC-530-AIMS Polyimide Foam
Subcategory: Polyimide; Thermoplastic
Material Notes: Description: SOLIMIDE® foams provide weight savings, improved handling/installation characteristics and enhanced durability compared to traditional insulation, resulting in lower operating and life cycle costs. In addition, the foams are extremely fire resistant and do not support combustion in normal atmospheres. Toxic gas, smoke generation and offgassing are virtually non-existent. These foam products are widely used in private, commercial, and military aircraft. SOLIMIDE® foams are specified and flying in Airbus, Boeing, Canadair, Boeing-Douglas, Hughes Helicopter, and Sikorsky Helicopter aircraft, among others. Meets AIMS 04-14-004, they are also approved for use in NASA systems. Information provided by degussa.
| Available Properties |
- Density
- Compressive Strength
- Compression Set
- Thermal Conductivity
- Maximum Service Temperature, Air
- Flammability Test
- Oxygen Index
- Acoustical Absorption Coefficient (1000Hz)
- Acoustical Absorption Coefficient (125 Hz)
- Acoustical Absorption Coefficient (2000 Hz)
- Acoustical Absorption Coefficient (250 Hz)
- Acoustical Absorption Coefficient (4000 Hz)
- Acoustical Absorption Coefficient (500 Hz)
- Noise Reduction Coefficient
- Smoke Emission at 4 Minutes
- Toxic Gas Generation
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|