Degussa AG Solimide® AC-550 Polyimide Foam

 

Subcategory: Polyimide; Thermoplastic

Material Notes:
Description: SOLIMIDE® foams provide weight savings, improved handling/installation characteristics and enhanced durability compared to traditional insulation, resulting in lower operating and life cycle costs. In addition, the foams are extremely fire resistant and do not support combustion in normal atmospheres. Toxic gas, smoke generation and offgassing are virtually non-existent. These foam products are widely used in private, commercial, and military aircraft. SOLIMIDE® foams are specified and flying in Airbus, Boeing, Canadair, Boeing-Douglas, Hughes Helicopter, and Sikorsky Helicopter aircraft, among others. Meets BMS 8-300, BAMS 544-006, DMS 2330, and they are also approved for use in NASA systems.

Information provided by degussa.

Available Properties
  • Density
  • Tensile Strength at Break
  • Compressive Strength
  • Compression Set
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Flammability Test
  • Oxygen Index
  • Acoustical Absorption Coefficient (1000Hz)
  • Acoustical Absorption Coefficient (125 Hz)
  • Acoustical Absorption Coefficient (2000 Hz)
  • Acoustical Absorption Coefficient (250 Hz)
  • Acoustical Absorption Coefficient (4000 Hz)
  • Acoustical Absorption Coefficient (500 Hz)
  • Flexibility
  • Noise Reduction Coefficient
  • Smoke Emission at 4 Minutes
  • Toxic Gas Generation
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。