Degussa AG Solimide® TA-301-DODI Polyimide Foam

 

Subcategory: Polyimide; Thermoplastic

Material Notes:
Description: SOLIMIDE® foams offer a unique combination of properties suited for demanding industrial environments. Because the foams retain their flexibility at cryogenic temperatures, they are utilized as expansion joints for cryogenic tanks, pipelines and wind tunnels. Very low outgassing makes SOLIMIDE® foams the choice for use in sensitive electronic, medical and analytical instruments. These products can be used at temperatures that would degrade other foams, allowing for use as insulation in ovens and other high temperature processes. SOLIMIDE® foams are used in a variety of applications from transportation to plant maintenance. They are environmentally "green," chemical and fire resistant, lightweight, durable, easy to install, and can be customized for any industrial situation. Meets U.S. Mil Spec DOD-I-24688.

Information provided by degussa.

Available Properties
  • Density
  • Tensile Strength at Break
  • Compressive Strength
  • Thermal Conductivity
  • Flammability Test
  • Flame Spread Index
  • Acoustical Absorption Coefficient (1000Hz)
  • Acoustical Absorption Coefficient (125 Hz)
  • Acoustical Absorption Coefficient (2000 Hz)
  • Acoustical Absorption Coefficient (250 Hz)
  • Acoustical Absorption Coefficient (4000 Hz)
  • Acoustical Absorption Coefficient (500 Hz)
  • Noise Reduction Coefficient
  • Toxic Gas Generation
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。