Degussa AG Trogamid® BX9723 30% Glass Fiber Reinforced Polyamide
Subcategory: Thermoplastic; Polymer
Material Notes: Description: TROGAMID BX9723 is a 30% glass fiber reinforced polyamide compound. The compound is suitable for the injection molding of extremely thermally resistant parts with high strength and hardness. Moldings of TROGAMID BX9723 show low shrinkage and low tendency to warp. Information provided by degussa.
| Available Properties |
- Density
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Ball Indentation Hardness
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|