Degussa AG Trogamid® BX9724 40% Glass Reinforced Nylon Blend

 

Subcategory: Nylon; Thermoplastic; Nylon 6-3; Polymer

Key Words: PA 6-3-T/XX, trimethyl hexamethylene diamine terephthalic acid

Material Notes:
Description: The TOGAMID® BX grades cover reinforced and non-reinforced blends based on PA 6-3-T and semi-crystalline polyamides. Non-reinforced blends are permanently transparent. Some blends have been developed in particular for manufacturing plastic-rubber composites. The special characteristics are:

  • high resistance to stress cracking
  • resistant to grease and fuels
  • good strength high hardness
  • very low mold shrinkage
  • very low tendency to warp
  • low moisture absorption
  • dimensionally stable even while absorbing water

The polyamide blends are especially suitable for the production of injection-molded parts subject to high thermal and mechanical stress. Thanks to their high stiffness moldings made from reinforced grades are appropriate for substituting cast metal parts, and are significantly lighter than these. Moldings exhibit outstanding surface qualities in spite of their high glass fiber content. TROGAMID® BX compounds can be combined with various rubber mixtures to produce plastic-rubber composite parts that are resistant to fuel and oil.

Specific Notes for this Material: Polymer blend consisting of amorphous and semi-crystalline polyamides, 40% glass fiber reinforced, with high tensile modulus for injection molding, dimensionally stable even while absorbing water; appropriate for substituting cast metal parts with plastic. Moldings exhibit outstanding surface qualities in spite of their high glass fiber content.

Information provided by degussa.

Available Properties
  • Density
  • Viscosity Test
  • Hardness, Shore D
  • Ball Indentation Hardness
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Charpy Impact Unnotched
  • Charpy Impact, Notched, Low Temp
  • Charpy Impact, Unnotched Low Temp
  • Charpy Impact, Notched
  • Tensile Creep Modulus, 1 hour
  • Tensile Creep Modulus, 1000 hours
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Comparative Tracking Index
  • CTE, linear 20°C
  • Melting Point
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Vicat Softening Point
  • Glass Temperature
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。