Degussa AG Trogamid® BX9728 Nylon 6-3 Compound for Plastic-Rubber Composite

 

Subcategory: Thermoplastic

Material Notes:
Description: The TOGAMID® BX grades cover reinforced and non-reinforced blends based on PA 6-3-T and semi-crystalline polyamides. Non-reinforced blends are permanently transparent. Some blends have been developed in particular for manufacturing plastic-rubber composites. The special characteristics are:

  • high resistance to stress cracking
  • resistant to grease and fuels
  • good strength high hardness
  • very low mold shrinkage
  • very low tendency to warp
  • low moisture absorption
  • dimensionally stable even while absorbing water

The polyamide blends are especially suitable for the production of injection-molded parts subject to high thermal and mechanical stress. Thanks to their high stiffness moldings made from reinforced grades are appropriate for substituting cast metal parts, and are significantly lighter than these. Moldings exhibit outstanding surface qualities in spite of their high glass fiber content. TROGAMID® BX compounds can be combined with various rubber mixtures to produce plastic-rubber composite parts that are resistant to fuel and oil.

TROGAMID BX compounds are oil- and fuel-resistant. They are suitable for manufacturing moldings with high strength and hardness that are subjected to high thermal stress. The mold shrinkage, warpage and moisture absorption are low.

Information provided by degussa.

Available Properties
  • Density
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Hardness, Shore D
  • Ball Indentation Hardness
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Charpy Impact Unnotched
  • Charpy Impact, Notched, Low Temp
  • Charpy Impact, Unnotched Low Temp
  • Charpy Impact, Notched
  • CTE, linear 20°C
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。